Title: Glass-ceramic crystallization from tailings of the Morille tungsten deposit, Spain
Author: Alfonso Abella, María Pura
Tomasa, Oriol
Garcia Vallès, Maite
Tarragó Aymerich, Mariona
Martínez Manent, Salvador
Keywords: Mineralogia
Vidre
Vitroceràmica
Jaciments minerals
Mineralogy
Glass
Glass-ceramics
Mineral deposits
Issue Date: 1-Apr-2022
Publisher: Elsevier B.V.
Abstract: The potential of the tailings from the Morille scheelite-bearing calc-silicate deposit as a commercial raw material for inert glass-ceramic was determined. Nucleation and crystal growth temperatures of glass were studied. The temperatures of maximum nucleation rate of the parent glass are 612 °C and 660 °C and crystal growth is at 776 °C and 1047 °C. At 776 °C a glass-ceramic of nepheline, wollastonite and akermanite is formed. In glasses treated at higher temperature nepheline becomes unstable and at 1047 °C a wollastonite-akermanite glass ceramic was obtained. The leaching tests show that the potentially toxic elements are effectively bound in the structure of the glass-ceramic, which can be considered inert.
Note: Versió postprint del document publicat a: https://doi.org/10.1016/j.matlet.2022.131694
It is part of: Materials Letters, 2022, vol. 312, num. 131694
URI: http://hdl.handle.net/2445/191680
Related resource: https://doi.org/10.1016/j.matlet.2022.131694
ISSN: 0167-577X
Appears in Collections:Articles publicats en revistes (Mineralogia, Petrologia i Geologia Aplicada)

Files in This Item:
File Description SizeFormat 
719093.pdf4.28 MBAdobe PDFView/Open


This item is licensed under a Creative Commons License Creative Commons