Title: | Sliding wear behavior of Fe-Al coatings at high temperatures |
Author: | Cinca i Luis, Núria Cygan, Slawomir Senderowski, C. Jaworska, Lucyna Dosta Parras, Sergi García Cano, Irene Guilemany, J. M. (José María) |
Keywords: | Compostos intermetàl·lics Revestiments Desgast mecànic Intermetallic compounds Coatings Mechanical wear |
Issue Date: | 1-Aug-2018 |
Publisher: | MDPI |
Abstract: | The medium and high temperature tribological behavior of different iron aluminide thermal spray coatings was investigated. Several powders synthesized through different routes (ball milling, self-decomposition, and self-propagating high-temperature sintering (SHS)) were evaluated. High heterogeneity of conventional High Velocity Oxygen Fuel (HVOF) coatings plays a vital role in their sliding performance, but as long as their integrity is preserved under high temperature oxidizing conditions, the wear rates are found to be acceptable, as it occurs in the case of ball milled Fe-40Al (at.%) powder. The friction phenomenon and wear mechanisms were analyzed in detail through the wear track morphology, contact surface, and friction coefficients. The occurrence of brittle phases in the sprayed coatings, which are also present when tested at high temperatures, appeared to be crucial in accelerating the coating failure. |
Note: | Reproducció del document publicat a: https://doi.org/10.3390/coatings8080268 |
It is part of: | Coatings, 2018, vol. 8, num. 268 |
URI: | http://hdl.handle.net/2445/158057 |
Related resource: | https://doi.org/10.3390/coatings8080268 |
ISSN: | 2079-6412 |
Appears in Collections: | Articles publicats en revistes (Ciència dels Materials i Química Física) Publicacions de projectes de recerca finançats per la UE |
Files in This Item:
File | Description | Size | Format | |
---|---|---|---|---|
690718.pdf | 3.71 MB | Adobe PDF | View/Open |
This item is licensed under a Creative Commons License