Amb motiu del tancament d'estiu, la validació de documents es reprendrà a partir del 28 d'agost de 2026. Disculpeu les molèsties.
Con motivo del cierre de verano, la validación de documentos se reanudará a partir del 28 de agosto de 2026. Disculpad las molestias
Due to the summer closure, document validation will resume starting August 28, 2026. We apologize for any inconvenience.

Tipus de document

Article

Versió

Versió publicada

Data de publicació

Llicència de publicació

cc-by (c) Tortora, Pietro C.D. et al., 2022
Si us plau utilitzeu sempre aquest identificador per citar o enllaçar aquest document: https://hdl.handle.net/2445/183795

Effect of Temperature and Humidity on the Synthesis of Alkali-Activated Binders Based on Bottom Ash from Municipal Waste Incineration

Títol de la revista

Director/Tutor

ISSN de la revista

Títol del volum

Resum

Weathered bottom ash (WBA) from municipal solid waste incineration is a calcium aluminosilicate-rich material mainly used in construction and civil engineering as a secondary aggregate. However, its use is also being considered as a precursor in the manufacture of alkali-activated binders (AA-WBA). This preliminary research aimed to deepen understanding of the potential use of WBA (>8 mm fraction) as the sole precursor of alkali-activated binders. To gain better knowledge of this material, the physicochemical, mechanical, and environmental properties of AA-WBA binders were evaluated. In addition, the effect of curing temperature (25 °C, 45 °C, 65 °C, and 85 °C) and humidity conditions (oven and climate chamber) were assessed. The results of this study revealed that temperature and humidity conditions play a fundamental role during the early formation stages of AA-WBA binders. Maximum compactness and compressive strength (29.8 MPa) were obtained in the sample cured at 65 °C in the oven and room humidity. At higher temperatures (85 °C), a substantial decrease in mechanical strength (21.2 MPa) was observed due to a lower cohesion of the binder phases. Curing in the climate chamber led to an increase in humidity, and therefore a decrease in compressive strength. Finally, lower porosity and longer curing time substantially decreased the heavy metals and metalloid leaching concentration of AA-WBA binders.

Citació

Citació

TORTORA, Pietro C.D., et al. Effect of Temperature and Humidity on the Synthesis of Alkali-Activated Binders Based on Bottom Ash from Municipal Waste Incineration. Sustainability. 2022. Vol. 14, num. 3, pags. 1848. ISSN 2071-1050. [consulted: 16 of August of 2026]. Available at: https://hdl.handle.net/2445/183795